Technical data sheet AQUAFIN®-OS 2K surface protection coating and waterproofing for concrete components
Material number
Package type
Colour
Units / pallet
Pc/package
201403001
30 kg, set (2 component)
Grey
40
1
A-component: 20 kg, bag
50
B-component: 10 kg, canister
Fields of application / waterproofing OS5b waterproofing for underground garages and parking garages against chloride exposure Protective coating against chloride attack and carbonation according to DIN 1504-2 Waterproofing of concrete structures below ground level in accordance with DIN 18533 Renovation and protection of concrete surfaces prone to cracking Waterproofing of construction and building joints For newbuild and renovation for interior and exterior use
Product features watertight High resistance to freeze/thaw cycles and de-icing salt attack CO2 and chloride barrier Water vapour permeable Can be painted and plastered For cementitious substrates Approved surface protection system according to OS 5b and EN 1504-2
SCHOMBURG GmbH & Co. KG · Aquafinstr. 2–8 · D-32760 Detmold (Germany) · Tel. +49-5231-953-00 · Fax +49-5231- 953-333 · schomburg.com 1/4
03/12/2025
Technical data sheet AQUAFIN®-OS Advantages Crack bridging at -20 °C Chloride-resistant UV-resistant Protects against carbonation
Technical Data Material properties Product components Base material Consistency Bulk density of fresh mortar Tensile adhesion strength DIN EN 1542 Rainproof Crack bridging DIN EN 1062-7
Water vapour permeability, SD value Classification of the reaction to fire in accordance with DIN EN 13501-1
2 component system Polymer-mortar combination Filler consistency approx. 1.7 kg/dm³ ≥ 0.8 N/mm² 4 hours At -20 °C and after 2000 h of UV weathering: 0.10 - 0.15 mm (1000 cycles) Procedure B DIN EN 1062-7, Class B2 Class sD > 5 m E
Mixing Mix ratio, component A Mix ratio, component B Mixing time Maturing time Water addition, maximum
1 weigh fraction (powder) 2 weight fractions (liquid) approx. 3 minutes approx. 2 minutes Max. 0.2 l per 30 kg
Application Substrate/application temperature Pot life Method of application, max. layer thickness per application step Consumption after OS5b and EN 1504-2 Consumption pro m² and mm layer thickness Overcoat after
approx. 5 - 30 °C approx. 30 minutes 2mm approx. 5.5 kg/m² approx. 1.7 kg approx. 3 hours
Processing equipment Aids/tools Stirrer (approx. 500-700 rpm) Suitable mixing paddle Trowel Serrated or layer-thickness trowel Flat trowel Brush Spray equipment
Manual processing Can be trowelled off Applicable with a brush
Machine application AQUAFIN®-OS can be mechanically applied. For precise information, see the additional Technical Information No. 43.
SCHOMBURG GmbH & Co. KG · Aquafinstr. 2–8 · D-32760 Detmold (Germany) · Tel. +49-5231-953-00 · Fax +49-5231- 953-333 · schomburg.com 2/4
Technical data sheet AQUAFIN®-OS Suitable substrate Old, firmly adhering bituminous substrates Concrete with a tensile adhesion strength of 1.5 N/mm² Masonry work Plasters P II and P III Cement-based screed (CT) All substrates in accordance with DIN 18535, DIN 18531, DIN 18533
Preparing the substrate Requirement for substrate 1. Even 2. Free of adhesion inhibiting substances 3. Sealed in the surface 4. Pore open 5. Load-bearing 6. Extensively fully grouted
Preparing the surface 1. Old, firmly adhering bituminous substrates must be covered with a scratch coat and overcoated after drying out completely. 2. In the case of substrates damaged by de-icing salt, the substrate must be removed down to the neutral area, e.g. by means of milling, etc. 3. On uneven substrates, pre-sealing can also take place with ASOCRET-M30. 4. Pre-moisten the dry substrate so that it is matt damp at the time of application. 5. Extremely absorbent and slightly sandy substrates must be primed with AQUAFIN-Primer. 6. Moisture penetration from the rear and intermittent moisture loading from the negative side must be avoided. 7. For waterproofing with moisture penetration from the rear, we recommend pre-sealing with AQUAFIN-1K-PLUS or ASODUR-SG3-thix.
Application Mixing 1. Put the liquid component into a clean mixing bucket and mix with the powder component to produce a homogeneous, lump-free mass. 2. The mixing time is ca. 3 minutes. 3. After a settling period of ca. 2 minutes, thoroughly homogenise the compound again. 4. Depending on the application technique (e.g. application by screen or spray technique), do not add more water than specified under “Technical Data > Mix > Water addition, maximum”. Water is added after mixing.
Application 1. Apply AQUAFIN®-OS as scratch coat and contact layer before first application. 2. Immediately afterwards, the first layer of sealant is applied wet-on-wet. 3. The second application step (and following) can take place when the first application step can no longer be damaged by reworking. (see “Technical Data > Application”) 4. The waiting time between layers depends on temperature, humidity and other ambient conditions.
Cleaning tools Clean tools thoroughly with water after use.
Storage conditions Storage Store in a cool and dry place. Min. 12 months in the original canister. Promptly use opened container.
SCHOMBURG GmbH & Co. KG · Aquafinstr. 2–8 · D-32760 Detmold (Germany) · Tel. +49-5231-953-00 · Fax +49-5231- 953-333 · schomburg.com 3/4
Technical data sheet AQUAFIN®-OS Notes Protect surfaces that are not to be treated from the effects of AQUAFIN®-OS! AQUAFIN®-OS as a surface coating must not be exposed to point or linear loads. AQUAFIN®-OS may be plastered and coated with vapour permeable, solvent-free dispersion facade paints or dispersion silicate paints (not pure silicate paints). Silicon resin paints and acrylate-based paints may also be used. On PVC, gunmetal, and stainless steel flanges, ASO®-Dichtmanschetten or alternatively ADF®-Pipe-Gasket must be installed without voids or wrinkles and integrated seamlessly into the waterproofing. In case of strong sunlight, work against the movement of the sun in shaded areas. Direct contact with metals such as copper, zinc, and aluminium must be avoided by means of a pore sealed primer. A pore-sealed primer is produced via 2 application steps using ASODUR®-GBM (see technical data sheet). In rooms with high humidity and/or insufficient ventilation (e.g. water containers), dropping below the dew point (condensation formation) may occur on the surface. This must be avoided by taking suitable measures such as by using condensation dryers. Direct heating or uncontrolled blowing warm air is not permitted. The waterproofing must not be affected by water during binding. The effect of water from behind can lead to spalling in case of frost.
Observe applicable safety data sheet!
The rights of the buyer with regard to the quality of our materials are based on our terms and conditions of sale and delivery. Our technical advice team will be happy to advise you in the case of requirements that exceed the scope of the application described here. In order to be binding, a legally binding written confirmation is required. The product description does not release the user from a duty of care. Lay a test area in the event of uncertainty. This version becomes invalid in the event of a new version being issued.
SCHOMBURG GmbH & Co. KG · Aquafinstr. 2–8 · D-32760 Detmold (Germany) · Tel. +49-5231-953-00 · Fax +49-5231- 953-333 · schomburg.com 4/4