Technical data sheet ASO®-SEB Binder for screeds, quickly ready to receive tiles
Material number
Contents
Unit of quantity
Packaging
Colour
206544001
25
KG
Bag
Cement grey
Areas of application As binders for creating rapid setting cement-based screeds As binder for producing bonded screeds, separating layer or as floating screed on an insulating layer Heated and unheated design For interior and exterior use
Product features Cementitious binder Rapid setting Quality up to CT-C50-F7 in accordance with DIN EN 13813
Advantages rapid construction progress High strengths possible Can be heated and tiled soon
SCHOMBURG GmbH & Co. KG · Aquafinstr. 2–8 · D-32760 Detmold (Germany) · Tel. +49-5231-953-00 · Fax +49-5231- 953-333 · schomburg.com 1/5
19/05/2025
Technical data sheet ASO®-SEB Technical Data Material properties Base material Consistency Heating, screed after
Special cement Additive Powdered after 3 days
Mixing Mix ratio, component A Mix ratio, aggregate Mixing time Water addition
1 weight proportion approx. 4 - 5 weight proportion approx. 2 - 3 minutes ca. 6 l - 7,5 l
Application Substrate temperature Pot life Mixing method, machines, tools Foot traffic after Ready for covering with tiles Application temperature Overcoat after Hardening time / full resilience
approx. 5 - 25 °C approx. 45 minutes Forced paddle mixer approx. 24 hours approx. 24 hours approx. 5 - 25 °C approx. 24 hours approx. 7 days
SCHOMBURG GmbH & Co. KG · Aquafinstr. 2–8 · D-32760 Detmold (Germany) · Tel. +49-5231-953-00 · Fax +49-5231- 953-333 · schomburg.com 2/5
Technical data sheet ASO®-SEB Material rate Material consumption rate according to the area of application
Minimum nominal thickness in accordance with DIN 18560
Layer thickness in accordance with grading curve
Processing equipment Machine application ASO®-SEB can be mechanically applied. For precise information, see the additional Technical Information No. 43.
Application Mixing recommendations for mixing and conveying machines 1. Half-fill the mixing drum with aggregate (0/8, approx. 15 scoops of 7 kg each), 50 kg ASO®-SEB and approx. 7.5 l water. 2. Add the remaining aggregate and then the remaining water. 3. The total mixing time is ca. 2 - 3 minutes. 4. Protect the fresh screed to prevent it drying out too rapidly, e.g. due to heat or draughts. 5. Tiles are ready for laying after one day if the following prerequisites are met: * Mix ratio of 1:4 parts by weight * Dry aggregate (DIN 4226; grading curve A8 - B8 close to B8; constant grading) * Water addition of 15 litres on 50 kg ASO®-SEB * Ambient and substrate temperature: +23 °C * Rel. humidity of 50% * Layer thickness of 5 cm 6. When it comes to other surface coverings, use the CM method to test the moisture content. 7. In the case of screeds that are required to satisfy a certain screed quality in accordance with DINEN13813, a performance test is necessary. This must be performed before starting the work.
SCHOMBURG GmbH & Co. KG · Aquafinstr. 2–8 · D-32760 Detmold (Germany) · Tel. +49-5231-953-00 · Fax +49-5231- 953-333 · schomburg.com 3/5
Technical data sheet ASO®-SEB Grading curve The adjacent diagrams show typical grading curves for aggregates frequently used for screed production. These are aggregates rich with fine parts, which require a greater quantity of water and binder in comparison to the optimum grading curve between A8-B8 close to B8. However, in accordance with investigations by the institute for building material testing and flooring research (“IBF”), use of such aggregates stands at almost 70% nationwide. Such aggregates are generally good to apply and smooth, but they require a greater quantity of water and binding agent in order to achieve similar strengths as with optimum grains. Our investigations with the adjacent typical representatives of aggregates rich with fine parts have shown that ASO-SEB in conjunction with grading curves around C8 and above can be used to produce good screeds if the formula is correspondingly adjusted (binder and added water).
Cleaning tools Clean tools thoroughly with water after use.
Storage conditions Storage Store in a cool and dry place. Min. 6 months in the original canister. Promptly use opened container.
Disposal Product residues can be disposed of in accordance with disposal code AVV 17 01 01.
Notes Do not add any additives and substances! Observe the technical data sheets of the products mentioned before starting work. For use in areas with inadequate aggregate quality or where storage of the mortar components is not possible or desirable, the ASO®-SEM / ASO®-EZ4-PLUS pre-blended dry mortars are available! A moisture measurement must be carried out using the CM method to assess whether it is ready to receive. Low temperatures, high humidity and heavy layer thicknesses delay hardening, drying and extend the time until ready to receive tiles. (Also see the BEB data sheet “Building climate preconditions for drying screeds”). Tests showed that the crystalline binding of the water is slower at low temperatures (+5 to +10°C), meaning that the screed was only ready to receive tiles after a longer period of time! Water that is pressed out of the surface of the screed indicates excessive water or aggregate addition (more than 3.3: 1 volume – parts, equates to approx. 5: 1 parts by weight), an incorrect grading curve or inadequate mixing. A consequence of this will be a crumbling surface! The quality of the aggregate used is partly decisive for the properties of the screed produced with it. Aggregate after DIN 4226 should be used with a constant grading curve between A and B close to B after DIN 1045. If aggregates with other grain distributions are used, a greater quantity of binder may be required. Aggregates with a grading curve between B and C after DIN 1045 require a higher proportion of ASO®-SEB. The grain size distributions that should be used with different layer thicknesses are available in the “Layer thickness in accordance with grading curve” table. ASO®-SEB can crystalline bind approx. 25% of its weight to water. Water quantities that exceed this volume must evaporate and therefore delay the readiness to receive tiles and boards! If the surface of the screed cannot be closed sufficiently when rubbed, this indicates that the proportion of fines in the aggregate is too low. A higher quantity of ASO®-SEB is required to replace the missing proportion of fines! If moisture rises from the substrate, effective waterproofing is essential prior to laying the screed! The installation location must be ventilated. However, draughts and direct solar radiation should be avoided during application and the hardening process. The indoor temperature and floor temperature must be at least +5°C during application, and during the following week! Air dehumidifiers may not be used during the first 3 days! Do not add any other cement or binder! Border, field, building separation and movement joints should be carried over to or installed at the designated location; suitable means (e.g. edge strips) should be used to detach them!
Relevant regulations Planning, inspection of substrates and building site circumstances, laying, grouting and subsequent care of the work must be done in accordance with the relevant DIN standards and recognised rules of technology (e.g. the ZDB Data sheets of the Zentralverband Deutsches Baugewerbe e.V.(German construction Association) in the latest version.
SCHOMBURG GmbH & Co. KG · Aquafinstr. 2–8 · D-32760 Detmold (Germany) · Tel. +49-5231-953-00 · Fax +49-5231- 953-333 · schomburg.com 4/5
Technical data sheet ASO®-SEB Observe applicable safety data sheet! GISCODE: ZP1
The rights of the buyer with regard to the quality of our materials are based on our terms and conditions of sale and delivery. Our technical advice team will be happy to advise you in the case of requirements that exceed the scope of the application described here. In order to be binding, a legally binding written confirmation is required. The product description does not release the user from a duty of care. Lay a test area in the event of uncertainty. This version becomes invalid in the event of a new version being issued.
SCHOMBURG GmbH & Co. KG · Aquafinstr. 2–8 · D-32760 Detmold (Germany) · Tel. +49-5231-953-00 · Fax +49-5231- 953-333 · schomburg.com 5/5